Fomapan 200@160 in NUCLEOL BF200 2%A+1,5%B
FILM SIZE
120/220
EXPOSURE INDEX
160
DEVELOPER
Ornano NUCLEOL BF200
DILUTION
2%A+1,5%B
TEMPERATURE (° C)
25
AGITATION
Every 60 sec.
Primo minuto agitazione continua, poi 4 inversioni ogni 60 sec